China GH5188 (H188) Cobalt-Based Superalloy Composition Analysis - China Supplier China GH5188 (H188) Cobalt-Based Superalloy Composition Analysis - China Supplier China GH5188 (H188) Cobalt-Based Superalloy Composition Analysis - China Supplier China GH5188 (H188) Cobalt-Based Superalloy Composition Analysis - China Supplier China GH5188 (H188) Cobalt-Based Superalloy Composition Analysis - China Supplier

GH5188 (H188) Cobalt-Based Superalloy Composition Analysis

Price:174
Industry Category: Metallurgy & Minerals
Product Category:
Brand: GH5188
Spec: GH5188


Contact Info
  • Add:上海市松江工业园区沪松公路, Zip: 201600
  • Contact: 李青
  • Tel:17749772286
  • Email:1036395561@qq.com

Other Products

Description
Additional Information

GH5188 Overview

GH5188 alloy is a solid-solution strengthened cobalt-based superalloy, primarily reinforced by carbides. Compared to nickel-based superalloys, this alloy offers superior creep resistance, thermal corrosion resistance, thermal fatigue resistance, and high-temperature strength. In the 1980s, GH5188 alloy was used in components such as vortex plates and flame guides for the WoZhou-8 aero-engine. Currently, it is selected for manufacturing high-temperature parts like combustion chamber inner walls, outer walls, and sealing strips in certain aero-engines. As a wrought cobalt-based superalloy, GH5188 has a simple microstructure. Due to the stability of carbides, they do not fully dissolve into the matrix during solution treatment, and the strengthening phases that precipitate during aging tend to over-age further during service, making aging treatment unsuitable. Cold-rolled strip is one of the common products of GH5188 alloy. The alloy raw material is smelted into ingots, then undergoes homogenization, cogging forging, hot rolling, multiple passes of cold rolling, and intermediate annealing, finally delivered in the solution-treated condition.

GH5188 Chemical Composition



Ni


W

Fe

B

La

0.05~0.15

20.0~24.0

20.0~24.0

Bal.

13.0~16.0

≤3.0

≤0.015

0.03~0.12

Mn

Si

P

S

Ag

Bi

Pb


Not more than

≤1.25

0.20~0.50

0.020

0.015

0.0010

0.0001

0.0010

0.07

GH5188 Mechanical Properties:

Product Form

Tensile Properties

Stress Rupture Properties

Hardness HV

Other Properties

θ/℃

σP0.2/MPa

σb/MPa

δ5/%

θ/℃

σ/MPa

t/h

δ5/%

Not less than

Not less than

Medium Plate

20

380

860

45

815
927

165
76

23
23

10
15

282

Grain size ≥ Grade 4

Thin Sheet

20
650

380
250

860
620

45
50

927

76

23

15

-

Bending, Oxidation Resistance, Grain Size

GH5188 Thermal Fatigue Performance

The initial melting point temperature range of the alloy is 1200~1210°C, with the initial melting phase being M23C6. After a homogenization process of 1180°C×20h, the eutectic structure is eliminated, dendritic segregation is reduced, and a more uniform microstructure is obtained.

After heat treatment at 1160°C×1h, the as-rolled microstructure experiences rapid grain growth, during which the M23C6 in the alloy dissolves into the matrix and disappears.

At low temperatures, thermal fatigue cracks propagate along the carbide interfaces, while at high temperatures, cracks extend by the interconnection of oxidation pores. Prolonged holding at the upper cyclic temperature limit at high temperatures facilitates the formation of a dense oxide layer, improving the alloy's thermal fatigue performance. However, excessive holding time leads to the formation of numerous oxidation pores on the surface, reducing fatigue performance. Heat treatment at 1175°C×75min+1000°C×8h can delay crack initiation with almost no effect on crack propagation rate. The above is an introduction to GH5188 cobalt-based alloy material.

Available in various specifications including plates, bars, strips, wires, discs, ring blanks, and ring forgings. Bars are supplied in forged-rolled condition, surface ground or turned; discs and ring blanks are supplied in forged condition; rings are supplied in solution-treated condition; plates are supplied after solution treatment, alkali-acid pickling, straightening, and edge trimming; strips are delivered cold-rolled, solution-treated, and descaled; wires are supplied in solution-pickled coil or straight form, or solution-treated straight fine-ground condition.

Industry Category Metallurgy & Minerals
Product Category
Brand: GH5188
Spec: GH5188
Stock:
Origin: China / Shanghai / Songjiangqu
About Toocle.com - Partner Programme - Old Version
Copyright © Toocle.com. All Rights Reserved.
(浙)-经营性-2023-0192